Polymer Property : Thermal Conductivity = 3.70 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.533 W/m-K
3.70 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Duratron® PAI T4501 Polyamide-imide, compression molded bearing grade (ASTM Product Data Sheet)
Thermal Conductivity 0.533 W/m-K
3.70 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet)