Thermal Properties Metric English Comments
Thermal Conductivity 0.488 W/m-K
3.39 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 15 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 0.488 W/m-K

@Temperature 500 °C
3.39 BTU-in/hr-ft²-°F

@Temperature 932 °F
Sharadaa Ceramics Sharada LTM 1.5 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Thermal Conductivity 0.489 W/m-K
3.39 BTU-in/hr-ft²-°F
Resinlab® EP11HT Gray Filled Epoxy Adhesive
Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..