Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.4531 W/m-K | 3.140 BTU-in/hr-ft²-°F | |
UBE UPIMOL® S High Heat Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |