Polymer Property : Thermal Conductivity = 291 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 42.0 W/m-K
291 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS179 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 42.0 W/m-K
291 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 147-31E Sintered Reaction Bonded Silicon Nitride (Si3N4)
Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met..
Thermal Conductivity 42.0 W/m-K
291 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4)
Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met..
Thermal Conductivity 42.0 W/m-K
291 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 147-1E Silicon Nitride
Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradynes ..