Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 28.8 W/m-K | 200 BTU-in/hr-ft²-°F | |
Conforma Clad WC 210 Tungsten Carbide-Nickel Cladding Conforma Clad is a targeted wear solution applied to vulnerable surfaces of a component. The wear protection is delivered via a proprietary cloth or slurry, ranging from 0.020" to 0.120" thick.If a.. |
|||
Thermal Conductivity | 28.8 W/m-K @Temperature 1000 °C |
200 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |