Thermal Properties Metric English Comments
Thermal Conductivity 27.7 W/m-K
192 BTU-in/hr-ft²-°F
SGL Carbon Group EK 204 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Thermal Conductivity 27.7 W/m-K
192 BTU-in/hr-ft²-°F
CeramTec 771 94% Alumina (Al2O3)
Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America.