Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 2544 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 366.6 W/m-K
2544 BTU-in/hr-ft²-°F
Cadi 150 Copper Alloy
A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electr..