Thermal Properties Metric English Comments
Thermal Conductivity 23.69 W/m-K
164.4 BTU-in/hr-ft²-°F
Crucible Steel 430F Stainless Steel
Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o..