Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 23.1 W/m-K | 160 BTU-in/hr-ft²-°F | perpendicular to c-axis |
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |