Thermal Properties Metric English Comments
Thermal Conductivity 322 W/m-K
2230 BTU-in/hr-ft²-°F
OMG Americas GlidCop® AL-60 Dispersion Strengthened Copper
GlidCop® AL-60 is copper that is dispersion strengthened with 1.1 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum o..
Thermal Conductivity 321 W/m-K
2230 BTU-in/hr-ft²-°F
Cytec Thornel® P-100 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..
Thermal Conductivity 322 W/m-K
2230 BTU-in/hr-ft²-°F
CMW® 328 Copper Alloy
CMW® 328 material is a high strength, high conductivity copper base alloy. CMW® 328 is heat treatable. Optimum mechanical and physical properties of CMW® 328 material are developed by heat treatm..