Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 220 W/m-K | 1530 BTU-in/hr-ft²-°F | |
Poco Graphite SUPERSiC® Si Silicon Carbide The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for.. |
|||
Thermal Conductivity | 220 W/m-K | 1530 BTU-in/hr-ft²-°F | |
Poco Graphite SUPERSiC® Si-3C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 75 µm CVD SiC coating, sealing off the porosity.Uses: Ideal for high-temperature vacuum CVD systemsInformation provided by Poc.. |
|||
Thermal Conductivity | 220 - 230 W/m-K | 1530 - 1600 BTU-in/hr-ft²-°F | z direction |
MarkeTech Cu/Mo/Cu 1:1:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Thermal Conductivity | 220 - 250 W/m-K | 1530 - 1740 BTU-in/hr-ft²-°F | |
MarkeTech Mo50Cu Moly/Copper Heat Sink Material MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivit.. |
|||
Thermal Conductivity | 220 - 250 W/m-K | 1530 - 1740 BTU-in/hr-ft²-°F | |
MarkeTech WCu25 Tungsten Copper Alloy Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Thermal Conductivity | 220 W/m-K | 1530 BTU-in/hr-ft²-°F | Typical |
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
Thermal Conductivity | 220 W/m-K | 1530 BTU-in/hr-ft²-°F | |
MMCC Al/SiC 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Thermal Conductivity | 220 W/m-K | 1530 BTU-in/hr-ft²-°F | |
MMCC Al/SiC Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Thermal Conductivity | 220 W/m-K | 1530 BTU-in/hr-ft²-°F | |
CMW® ELKONITE® 10W3 Copper Tungsten RWMA Class 11 Electrical contacts resistant to arcing, power transformer switches, resistance / projection welding electrodes, and EDM electrodesInformation provided by CMW Inc. |
|||
Thermal Conductivity | 220 W/m-K | 1530 BTU-in/hr-ft²-°F | |
CMW® THERMKON® 83 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Thermal Conductivity | 220 W/m-K | 1530 BTU-in/hr-ft²-°F | |
Poco Graphite SUPERSiC® Si-8C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 200 µm CVD SiC coatingUses: Ideal for optical and lithography componentsInformation provided by Poco Graphite |