Thermal Properties Metric English Comments
Thermal Conductivity 22.5 W/m-K

@Temperature 700 °C
156 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 22.5 W/m-K

@Temperature 700 °C
156 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 22.5 W/m-K

@Temperature 700 °C
156 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 22.5 W/m-K

@Temperature 700 °C
156 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 22.5 W/m-K

@Temperature 700 °C
156 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 22.5 W/m-K

@Temperature 700 °C
156 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 22.5 W/m-K

@Temperature 700 °C
156 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 22.5 W/m-K

@Temperature 700 °C
156 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 22.5 W/m-K

@Temperature 700 °C
156 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..