Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 31.0 W/m-K | 215 BTU-in/hr-ft²-°F | |
Goodfellow Platinum 90/Iridium 10 Alloy The alloy has been used in "non-standard" thermocouples, electrical contacts and for electrodes in medical research. The alloy is harder and mechanically stronger than Platinum.Information provided .. |
|||
Thermal Conductivity | 31.0 W/m-K | 215 BTU-in/hr-ft²-°F | ASTM-C408 |
CoorsTek PlasmaPure-UC™ 99.9% Alumina |
|||
Thermal Conductivity | 31.0 W/m-K | 215 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories 99 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
Thermal Conductivity | 31.0 W/m-K | 215 BTU-in/hr-ft²-°F | hardness of 56 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |