Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 29.275 - 33.46 W/m-K @Temperature 20.0 °C |
203.16 - 232.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
International Mold Steel Porcerax II Sintered, Porous Mold Steel Description: Porcerax II is a sintered, porous metal with porosity in the range of 20 to 30% by volume. A system of interconnected pores with an average diameter of 7 or 20 micron is dispersed throu.. |