Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.140 - 0.390 W/m-K | 0.972 - 2.71 BTU-in/hr-ft²-°F | Average value: 0.284 W/m-K Grade Count:5 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |