Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.385 W/m-K | 2.67 BTU-in/hr-ft²-°F | |
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M |