Thermal Properties Metric English Comments
Thermal Conductivity 0.335 - 0.377 W/m-K
2.32 - 2.61 BTU-in/hr-ft²-°F
Polikim EFALON® C-15 PTFE, 15% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..