Polymer Property : Thermal Conductivity = 2.32 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 2.32 W/m-K
16.1 BTU-in/hr-ft²-°F
Atom Adhesives AA-DUCT 904 Epoxy Adhesive
AA-DUCT 904 is a single component, heat curing, conductive epoxy that was designed for ease in handling. This high performance conductive epoxy cures quickly at elevated temperatures making it ideal..