Polymer Property : Thermal Conductivity = 2.22 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 2.22 W/m-K
15.4 BTU-in/hr-ft²-°F
in-plane, ø80*3mm discs; ISO 22007-2
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific)
Thermally conductive mineral filled PPS FR compound