Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-10 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-25 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-15 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-20 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-3 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-6 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |