Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 189 W/m-K @Temperature 20.0 - 400 °C |
1310 BTU-in/hr-ft²-°F @Temperature 68.0 - 752 °F |
|
Hogen Duralloy H10W 75 Tungsten/25 Copper PM Metal Composite RWMA Class 11.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 11 Cu-W (a hard.. |