Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 257.7 W/m-K | 1788 BTU-in/hr-ft²-°F | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Thermal Conductivity | 257.7 W/m-K | 1788 BTU-in/hr-ft²-°F | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Extra Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Thermal Conductivity | 257.7 W/m-K | 1788 BTU-in/hr-ft²-°F | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Thermal Conductivity | 257.7 W/m-K | 1788 BTU-in/hr-ft²-°F | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Spring 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |