Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.5 - 17.5 W/m-K | 115 - 121 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories Slab SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |