Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 167 W/m-K | 1160 BTU-in/hr-ft²-°F | |
Alcoa UltrAlloy® 6020-T651 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
Thermal Conductivity | 167 W/m-K | 1160 BTU-in/hr-ft²-°F | |
CMW® THERMKON® 68 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |