Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.95 W/m-K | 117.6 BTU-in/hr-ft²-°F | |
TIMET 75A CP Titanium (ASTM Grade 4) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features.. |