Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 21.6 W/m-K @Temperature 500 °C |
150 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 100 °C |
150 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Crucible Steel CPM® 9V® Tool Steel CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced.. |
|||
Thermal Conductivity | 21.6 W/m-K | 150 BTU-in/hr-ft²-°F | |
Astro Met ZTA 96 Zirconia Toughened Alumina General Description:ZTA-96 is a zirconia toughened alumina ceramic that exhibits excellent wear and corrosion resistance along with high strength and toughness. Astro Met has developed ZTA-96 zircon.. |