Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 14.2 - 15.8 W/m-K | 98.5 - 110 BTU-in/hr-ft²-°F | as built |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |