Polymer Property : Thermal Conductivity = 1388 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 130.0 - 200.0 W/m-K
902.2 - 1388 BTU-in/hr-ft²-°F
ALIMEX 2017A T451 Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then naturally aged.