Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 138 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 138 W/m-K
958 BTU-in/hr-ft²-°F
Hogen HM3000 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a l..
Thermal Conductivity 138 W/m-K
958 BTU-in/hr-ft²-°F
Mi-Tech Metals HD18 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high therm..
Thermal Conductivity 138 W/m-K
958 BTU-in/hr-ft²-°F
Alcoa Deltalloy® 4032-T651 Aluminum
Weldability = B; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = C (A = best; E = worst). General 4032 characteristics and uses: Good machinability and drilling characterist..
Thermal Conductivity 138 W/m-K
958 BTU-in/hr-ft²-°F
Alcoa Deltalloy® 4032-T86 Aluminum
Weldability = B; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = C (A = best; E = worst). General 4032 characteristics and uses: Good machinability and drilling characterist..