POLYMER SEARCH
Polymer Property : Thermal Conductivity = 13.3 BTU-in/hr-ft²-°F
Polymer Property :
Thermal Conductivity =
13.3 BTU-in/hr-ft²-°F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Thermal Conductivity
1.92
W/m-K
13.3
BTU-in/hr-ft²-°F
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive
Self-extinguishing version of 3748 and Meets UL 1410 requirementsInformation provided by 3M