Polymer Property : Thermal Conductivity = 1260 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 182 W/m-K

@Temperature 20.0 - 400 °C
1260 BTU-in/hr-ft²-°F

@Temperature 68.0 - 752 °F
Hogen Duralloy H30W 80 Tungsten/20 Copper PM Metal Composite
RWMA Class 12.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is ..