Polymer Property : Thermal Conductivity = 12.7 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.83 W/m-K

@Temperature 538 °C
12.7 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Pyrotek Pyrocast ZEAL Refractory Shapes
Aggregate Base: MulliteApplicationsDoor sill Furnace ramp Crucible bottom / lining Information provided by Pyrotek.