Thermal Properties Metric English Comments
Thermal Conductivity 17.240 W/m-K

@Temperature 538 °C
119.64 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Crucible Steel 20 Cb Plus Stainless Steel
Crucible 20 Cb Plus is a non-hardenable stabilized stainless steel with exceptional resistance to sulfuric, phosphoric, and nitric acid. This grade also has good resistance to stress corrosion crack..