Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 1145.1 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 165.01 W/m-K
1145.1 BTU-in/hr-ft²-°F
ALIMEX AMP 8000 Aluminum Plate
AMP 8000 offers higher strength levels, good machinability and dimensional stability. Its tensile strength is up to 40% higher than AlZn5.5MgCu (7075). Moulding, (Prototypes) injection moulds, Jig ..
Copyright © lookpolymers.com All Rights Reserved