Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 15.91 W/m-K | 110.4 BTU-in/hr-ft²-°F | |
Eagle Brass 64725 MAX251C, 1/2 Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Thermal Conductivity | 15.91 W/m-K | 110.4 BTU-in/hr-ft²-°F | |
Eagle Brass 64725 MAX251C, Extra Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Thermal Conductivity | 15.91 W/m-K | 110.4 BTU-in/hr-ft²-°F | |
Eagle Brass 64725 MAX251C, Extra Spring Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Thermal Conductivity | 15.91 W/m-K | 110.4 BTU-in/hr-ft²-°F | |
Eagle Brass 64725 MAX251C, Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Thermal Conductivity | 15.91 W/m-K | 110.4 BTU-in/hr-ft²-°F | |
Eagle Brass 64725 MAX251C, Spring Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |