Polymer Property : Thermal Conductivity = 105.5 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 105.5 W/m-K
732.2 BTU-in/hr-ft²-°F
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy
This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65%..