Thermal Properties Metric English Comments
Thermal Conductivity 120 - 150 W/m-K
833 - 1040 BTU-in/hr-ft²-°F
Temper T651
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Thermal Conductivity 135 - 150 W/m-K
937 - 1040 BTU-in/hr-ft²-°F
temper T651
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..