Polymer Property : Thermal Conductivity = 1.75 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.252 W/m-K
1.75 BTU-in/hr-ft²-°F
ASTM E1530-11
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet)
Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam
Thermal Conductivity 0.252 W/m-K
1.75 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet)
Thermal Conductivity 0.252 W/m-K
1.75 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
Thermal Conductivity 0.252 W/m-K
1.75 BTU-in/hr-ft²-°F
ASTM C177
Quantum Polysulfone
Information provided by Quantum Advanced Engineering Plastics