Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.73 W/m-K | 12.0 BTU-in/hr-ft²-°F | ASTM D177 |
Manifattura Cattaneo VESPEL® SP22 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 1.73 W/m-K | 12.0 BTU-in/hr-ft²-°F | ASTM C177 |
Techmer ES HiFill® PPS 0237 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
Thermal Conductivity | 1.73 W/m-K | 12.0 BTU-in/hr-ft²-°F | ASTM C177 |
Techmer ES HiFill® PPS 0334 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |