Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.58 W/m-K | 11.0 BTU-in/hr-ft²-°F | |
Mykroy/Mycalex MM 501 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide.. |