Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.04 W/m-K @Temperature 87.0 °C |
7.22 BTU-in/hr-ft²-°F @Temperature 189 °F |
|
Schott AF 45 Thin Borosilicate Glass AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc.. |
|||
Thermal Conductivity | 1.04 W/m-K | 7.22 BTU-in/hr-ft²-°F | |
Schott N-KF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 1.04 W/m-K | 7.22 BTU-in/hr-ft²-°F | |
Schott N-SF15 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 1.04 W/m-K | 7.22 BTU-in/hr-ft²-°F | |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |