Polymer Property : Thermal Conductivity = 0.979 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.141 W/m-K
0.979 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® T65 XF Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content
Thermal Conductivity 0.141 W/m-K
0.979 BTU-in/hr-ft²-°F
Melt
Covestro Desmopan® DP 1080A Polyurethane
injection molding gradefree from plasticizershard - soft systemsTechnical partsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covest..
Thermal Conductivity 0.141 W/m-K
0.979 BTU-in/hr-ft²-°F
Melt
Covestro Desmopan® DP 8798A Polyurethane
injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content