Polymer Property : Thermal Conductivity = 0.901 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.901 W/m-K
6.25 BTU-in/hr-ft²-°F
uncured
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive
AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o..