Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0600 - 0.120 W/m-K | 0.416 - 0.833 BTU-in/hr-ft²-°F | Average value: 0.0851 W/m-K Grade Count:6 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |