Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0760 - 0.830 W/m-K | 0.527 - 5.76 BTU-in/hr-ft²-°F | Average value: 0.129 W/m-K Grade Count:17 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |