Thermal Properties Metric English Comments
Thermal Conductivity 0.790 W/m-K

@Temperature 80.0 °C
5.48 BTU-in/hr-ft²-°F

@Temperature 176 °F
Z Direction; ASTM C518
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Features and Benefits:
Thermal Conductivity 0.790 W/m-K
5.48 BTU-in/hr-ft²-°F
Schott N-LAF36 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.790 W/m-K
5.48 BTU-in/hr-ft²-°F
Schott N-LASF41 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.790 W/m-K
5.48 BTU-in/hr-ft²-°F
Schott N-LASF9 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.790 W/m-K
5.48 BTU-in/hr-ft²-°F
Schott P-SF67 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.790 W/m-K
5.48 BTU-in/hr-ft²-°F
Schott N-LASF31a Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.790 W/m-K
5.48 BTU-in/hr-ft²-°F
ASTM C518
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic
RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe..
Thermal Conductivity 0.790 W/m-K
5.48 BTU-in/hr-ft²-°F
ASTM C518
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac
RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am..