Thermal Properties Metric English Comments
Thermal Conductivity 0.66992 W/m-K
4.6492 BTU-in/hr-ft²-°F
Cosmic Plastics E4940 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade
Data provided by the manufacturer.
Thermal Conductivity 0.66992 W/m-K
4.6492 BTU-in/hr-ft²-°F
Cosmic Plastics E486 lass Filled Epoxy Molding Compound, Electrical Grade
Data provided by the manufacturer.
Thermal Conductivity 0.66992 W/m-K
4.6492 BTU-in/hr-ft²-°F
Cosmic Plastics E4920 Mineral Filled Epoxy Molding Compound, Encapsulated Grade
Data provided by the manufacturer.
Copyright © lookpolymers.com All Rights Reserved