Polymer Property : Thermal Conductivity = 0.610 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 100 - 100 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.570 W/m-K Grade Count:4
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..