Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0663 W/m-K | 0.460 BTU-in/hr-ft²-°F | ASTM C177 |
Ensinger Tecapeek® XP-110 Compression Molded PEEK Compound, 45% Mineral Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |