Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0550 - 0.0640 W/m-K | 0.382 - 0.444 BTU-in/hr-ft²-°F | |
Beijing Evergrow Resources GFF-3 Glass Fiber Felt Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a.. |